This is the authors' abstract. We don't add key points for this paper.
An attempt was made to prepare the polymer fractions having extremely sharp molecular weight distribution (MWD), by using a successive solutional fractionation (SSF) method, in which a polymer‐lean phase was separated as a fraction from a polymer‐rich phase. For this purpose a large‐scale preparative SSF apparatus was constructed. Atactic polystyrene (PS) high‐density polyethylene (PE), and cellulose di‐ and tri‐acetates (CDA and CTA) were fractionated by SSF. The fractions isolated from a quasi‐binary mixture (polymer/solvent system) have the same MWD as that predicted by the computer simulation technique. Even under the conventional fractionation conditions (initial polymer volume fraction vop = ∼ 0.01, total number of fractions nt = 10 ∼ 20) the fractions with the ratio of the weight to number‐average molecular weight Mw/Mn less than 1.1 for PS, 1.2 for PE, 1.3 for CDA and 1.4 for CTA were obtained, with exception of a few initial fractions. The advantage of the SSF method was clarified over the conventional preparative methods such as gel permeation chromatography and the column fractionation method.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kamide et al. (1981) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: