Positron lifetime and Doppler broadening measurements have been done to study the α-induced defects in stainless steel SS 302 and polycrystalline cobalt. For stainless steel the samples have been thin and the effect of the presence of helium on defect kinetics has been avoided by allowing the 30 MeV alpha particles to pass through the samples. The presence of impurity (carbon) atoms in steel is found to play an important role in the trapping and detrapping of vacancies in the temperature range 200°C to 450°C. Formation of vacancy-impurity complexes and their dissociation around 500°C have been observed. A steady decrease of the positron parameters has been seen beyond 700°C and they attain those of the reference sample around 1000°C. While annealing alpha irradiated cobalt we find migration of vacancies and rearrangement of dislocation loops below 650 K and then dissolution around 900 K. Helium-vacancy complexes form in the region 600 to 1000 K, leading to the growth of the He-bubble above 1000 K. The trapping model analysis shows strong interaction between He and vacancy clusters in the temperature region 600 to 1000 K.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Mukhopadhyay et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: