Answers are grounded in this paper and cite their sources.
The photochemical deposition (PCD) technique for selenides is developed and applied to CdSe. In PCD, a substrate was held in an aqueous solution and was irradiated with a mercury lamp. The deposition solution for CdSe contained CdSO4, Na2SeO3, and Na2SO3. In the PCD processes, sulfite ions acted as a reducing agent under UV irradiation. The deposited films have nearly stoichiometric composition. The bandgap energy is in the range 1.85–1.9 eV for the as-deposited films and is decreased by about 0.1 eV by annealing at 300 °C. The annealed films have the cubic zincblende structure.
No takes yet. Share an insight, caveat, or question.
Ichimura et al. (2002) studied this question.