Spinel of composition has been synthesized by a combustion-aided procedure. The particles of the sample are single crystals of ca. 10 nm size as deduced from X-ray diffraction and transmission electron microscopy. Thermal treatment of the as-prepared sample at increasing temperature (400, 600, 700, 750, 900, 1000, and 1100°C) for different times (1, 3, or 24 h) leads to an increase of the particle size, which attains a value as high as 1560 nm after heating at 1100°C for 1 h. Electrochemical response of the heated samples as positive electrodes in a lithium cell has been studied at three rates (C/24, C, and 3C; where mA). At C/24 the discharge capacity measured at 4 and 4.8 V is not appreciably affected by the particle size. At C and 3C the discharge capacity measured at those voltages decreases as the particle size increases; a linear dependence has been found for particle sizes above 50 nm. On cycling we have found that the capacity fade also depends on the particle size; the larger the particles the less the capacity fade at the mentioned voltages.
No takes yet. Share an insight, caveat, or question.
Pascual et al. (2005) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: