Answers are grounded in this paper and cite their sources.
The diffusion layer thickness, δ, was measured as a function of time by a Mach‐Zehnder interferometer on a vertical cathode in CuSO 4 solution with and without an excess of H 2 SO 4 at current densities, i , up to 100 mA/cm 2 . The thickness δ increased linearly with t ½ up to the start of hydrogen gas evolution in CuSO 4 solutions with and without H 2 SO 4 ; in the presence of tenfold excess of H 2 SO 4 ,δ rapidly increased just before the gas evolution. At a constant cathodic charge, log δ decreased linearly with increasing log i in both solutions and δ is larger in pure CuSO 4 solution than in the presence of excess of H 2 SO 4 .
No takes yet. Share an insight, caveat, or question.
Tvarusko et al. (1971) studied this question.