Answers are grounded in this paper and cite their sources.
The melt spinning of a Pb-Bi-Te system alloy with Pyrex glass was investigated as a means of producing a superconducting long filament with high T c. Long filaments with T c higher than 10 K, having a mixed structure of the ε-phase, the bismuth phase and the tellurium phase were obtained from the molten state at 1500 K with a winding speed of 2.63 m/s. For example, a Pb45Bi40Te15 filament with T c of 10.2 K was 24 µm in diameter and was a ductile material with a tensile strength of 29 MPa and an elongation of 3.1%. A filament annealed at 573 K for 600 s had a high T c of 9.7 K and a high strength of 20 MPa. Severe heat treatment did not cause the growth of crystal grains of size 2000 Å. The lead, bismuth and tellurium were distributed homogeneously in the filament. The interface between the tellurium and the ε-phase is considered to play an important role in the enhanced T c.
No takes yet. Share an insight, caveat, or question.
Gotō et al. (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: