Answers are grounded in this paper and cite their sources.
In this study, based on designed Ti-50Ni, Ti-27Ni-23Nb, and Ti-27Ni-19Nb-4X (Ta and V) SMAs were prepared using arc melting. The microhardness and microstructure of the prepared alloys were examined. The optical microscope (OM) and Scanning Electron Microscopy (SEM) images can be noted that Nb, Ta, and V addition in substitution to nickel causes a change in the microstructure morphology of TiNi Shape Memory Alloy at room temperature. The microhardness results shown that when V and Ta elements were added to SMAs, the microhardness of the alloys was significantly increased. The microhardness value of equal atomic Ti-Ni SMA was found to 243 HV0.3. This value was determined to 354 HV0.3 in the Ti-27Ni-23Nb ternary SMA. By the addition of Ta into the Ti-Ni-Nb alloy, the microhardness value was enhanced to approximately 380HV, additionally, moreover, by adding Vanadium element to the ternary alloy, the microhardness was increased to about 500 HV.
No takes yet. Share an insight, caveat, or question.
Balci et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: