Mercuric telluride was synthesized and single crystals were prepared both in a horizontal capsule and by the Bridgman technique. The Hall coefficient R and the resistivity ρ were measured as a function of temperature and magnetic field. Above 250°K the material was intrinsic with an energy gap of around 0.02 ev and a mean density‐of‐states effective carrier mass of about 0.04 . Hall effect and mangetoresistance data indicated that at 300°K while . In the intrinsic temperature range, mobilities decreased with increasing temperature. At low temperatures R decreased markedly with magnetic induction even though R measured at low fields was independent of temperature for one of the ingots. In addition, the magnetoresistance fell far below a dependence at low temperatures. This behavior is characteristic of p‐type semiconductors in the transition temperature range between intrinsic and extrinsic conduction. In this transition temperature range is quite wide because of the low energy gap. Since all material prepared from the melt was p‐type, it seems that there is either a dominating acceptor impurity in all the samples or the maximum melting point of the compound does not occur at the stoichiometric composition.
No takes yet. Share an insight, caveat, or question.
Black et al. (1958) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: