The technique of spin-wave resonance has been employed to experimentally determine the spin-wave dispersion coefficient D for different compositions of nickel in iron. The results of this investigation indicate that for the fcc alloys (nickel-rich), the spin-wave dispersion coefficient decreases from its room-temperature value of 3.8×{}10^-27 erg cm² at 60-at.% Ni in Fe to a minimum of 2.7×{}10^-27 erg cm² at 45-at.% Ni in Fe. It then rises to a maximum of 6.5×{}10^-27 erg cm² at the Invar point, 27-at.% Ni in Fe. The spin-wave dispersion coefficient for the bcc alloy (iron-rich) taken at room temperature decreases linearly from its value of 5.0×{}10^-27 erg cm² at pure iron to a value of 2.7×{}10^-27 erg cm² at the Invar point. The shape of both the bcc and fcc plots are in agreement with a plot constructed from data obtained using the technique of small-angle neutron scattering. The Land\'e g factor has also been determined as a function of composition of nickel in iron. For the bcc material, g is a constant at 2.20 in the range 22-31-at.% Ni in Fe. For the fcc material, g varies from its value of 2.15 in the region 42-60-at.% Ni in Fe to a value of 1.79 at 33-at.% Ni in Fe and then rises to 2.00 near the Invar point. The complex spin-wave patterns that are often detected in Invar thin films of mixed crystalline structure have been attributed to the different magnetizations associated with each of the crystalline phrases.
No takes yet. Share an insight, caveat, or question.
Bauer et al. (1972) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: