Furfuryl alcohol was polymerized by trifluoroacetic acid in methylene chloride to give a colored polymer. This polymer possesses two main sequences in which the furan rings are connected by methylene groups (sequence 1) or by dimethylene ether groups (sequence 2). The polymer is not linear but highly branched, as detected by 1H and 13C NMR spectroscopy. Variations of the experimental conditions, such as the presence of air, the trifluoroacetic acid concentration, the reaction temperature and the solvent, do not allow a significant increase in the linear structure of the polymer. However, an increase in the acid concentration or an increase in temperature produce a decrease in the ether‐bridged structure (sequences 2).