Answers are grounded in this paper and cite their sources.
Acetylenic monomers containing indan and other groups ( 1a − m ) were polymerized with TaCl 5 - n -Bu 4 Sn catalyst to give high molecular weight polymers. Most polymers were soluble in common organic solvents including toluene and chloroform, and they afforded free-standing membranes by the solution casting method. The onset temperature of weight loss of the polymers were over 400 °C, indicating high thermal stability. Despite the absence of bulky spherical groups, polymethylated indan-containing polymer membranes showed extremely high gas permeability. In particular, the oxygen permeability coefficients of polymers having 1,1,3,3-tetramethylindan and either p -fluorophenyl or p, m -difluorophenyl groups ( 2b and 2e ) reached 17 900 and 18 700 barrers, respectively, which are even larger than that of the most permeable polymer known, poly(1-trimethylsilyl-1-propyne).
No takes yet. Share an insight, caveat, or question.
Hu et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: