Nickel-doped Zinc Oxide (Zn(1-x)Ni(x)O) nanoparticles have been synthesized by the chemical coprecipitation method. The structure and characteristic of synthesized Ni doped ZnO nanoparticles ware analyzed by X-ray diffraction (XRD) patterns. Crystallite sizes and lattice strain of all samples were calculated using the Scherrer’s formula, Uniform Deformation Model (UDM) and Halder-Wagner (H-W) method. X-ray diffraction analysis confirmed hexagonal cubic structure of Ni-doped ZnO nanoparticles. Also, the crystallite size of the nanoparticles reduces as the nickel concentration increase. The result showed the average crystallite size calculated by Scherrer’s formula (25-29 nm) was smaller than crystallite size using UDM method (51-63) the largest average crystallite size and H-W method (42-47 nm). The lattice strain increases with decreasing crystallite sizes value. The crystal size Ni- doped ZnO nanoparticles decreased with increasing dopant concentration.
No takes yet. Share an insight, caveat, or question.
Destalina et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: