This is the authors' abstract. We don't add key points for this paper.
The thermal conductivity λ has been measured in the temperature range 190–330 K and at pressures up to 1.0 GPa for the various phases of odd-numbered n-alkanes ranging from C9H20 to C19H40. We used the transient hot-wire technique. At 0.03 GPa, the thermal conductivity for the plastic crystal phase was about 0.2 W m−1 K−1 and showed no clear variation with chain length. For all n-alkanes the increase in λ at the liquid→plastic crystal phase transition was about 35%. At low pressures λ increased monotonically with increasing chain length for the low temperature phase. At pressures above 0.5 GPa and at 273 K the λ results of C9H20 and C11H24 indicate that these two substances transform into another, more close-packed, structure than that of the longer odd-numbered n-alkanes.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Forsman et al. (1984) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: