Answers are grounded in this paper and cite their sources.
In a Paleudult of Java Island, there was a clay mineral indicating a mixed layer mineral which gave 15.51 A peak (in the range of 14.63 A and 16.37 A) on Mg 2+ -air dry and a 20.55 A peak on Mg 2+ -glycerol solvation. On K - -saturation, the mineral showed an 11.87 A peak and this peak was continuous to 7.53 A. Furthermore, on sequential heating, the peak gradually shifted and finally shifted completely to 10.05 A at 550°C in X-ray diffraction (XRD). A peak of 7.53A was also observed in both Mg 2+ - and K + -saturated clays which disappeared after heating at 550°C. The objective of this study was to investigate the characteristics of this mineral. The 060 peak was 1.50 A and suggests the dioctahedral smectite. The Greene-Kelly test on the clay sample suggests beidellite. Formamide solvation that caused a swelling of the 7.53 A peak to 10.05 A suggests the presence of halloysite. The 5M NaOH treatment resulted in a collapse of the 7.53A peak and remained at a sharp peak of 15.50 A (in Mg 2+ -saturated clay). The presence of halloysite was also supported by a SiO 2 /Al 2 O 3 molar ratio of NaOH extractable materials. The NaOH treatment also resulted in an increase of the 11.87 A peak (in K + -saturated clay) to 13.49 A. According to the mineralogical and chemical properties of the clay sample we consider that the mineral is halloysite/beidellite mixed layer mineral.
No takes yet. Share an insight, caveat, or question.
Nurcholis et al. (1998) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: