We observed crack formation in transformation-processed Nb 3 Al wires at room temperature, the wire being bent with a small clamp fixture with a curvature. The polished cross-section parallel to the longitudinal axis was observed, using a high power optical microscope or a field-emission scanning electron microscope. The bend strain limit for microcrack formation is found, changing the radius of the curvature of the clamp. The bend strain limit was found to be around 0.3% for standard Nb 3 Al wires. This corresponds to the irreversible tensile strain limit of the I c characteristics determined with a 0.1 µV cm −1 criterion. Reduction of the barrier thickness should be avoided to keep to the bend strain limit. A new configuration of the Nb 3 Al wire is demonstrated to improve the bend strain limit. The filament is divided into segments in the transverse cross-section. The wire is fabricated by a double-stacking method. The bend strain limit is enhanced to about 0.85% for the wire surface; the equivalent strain of the outermost filament location is about 0.66%. A simple react and wind test for this wire was performed, where the wire experienced 0.86% bend strain. The degradation of J c was found to be very small.
No takes yet. Share an insight, caveat, or question.
Banno et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: