Answers are grounded in this paper and cite their sources.
The current investigation aims to study performance of geopolymer mortar reinforced with Multiwalled carbon nanotubes upon exposure to 200∘C to 1000∘C for 2 hrs. MWCNTs are doped into slag Geopolymer mortar matrices in the ratio of 0.0 to 0.4, % by weight of binder. Mortar composed of calcium aluminosilicate to sand (1:2), however, binder composed of 50% air cooled slag and 50% water cooled slag. Various water / binder ratios in the range of 0.114-0.129 used depending on the added MWCNT, while 6 wt., % sodium hydroxide used as an alkali activator. Results illustrate reduction in mechanical strength with temperature except specimens containing 0.1 and 0.2% MWCNT at 200∘C , while further increase in temperature leads to decrease in strength values of the resulting geopolymer mortar. Also, decrease in firing shrinkage with MWCNT up to 0.1% at all firing temperatures up to 500∘C is observed, however the shrinkage values increase with temperature up to 500∘C . Further increase on the firing temperature up to 1000∘C results in an increase in the volume due to expansion.
No takes yet. Share an insight, caveat, or question.
Khater et al. (2015) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: