The CuO x thin film photocathodes were deposited on F-doped SnO 2 (FTO) transparent conducting glasses by alternating current (AC) magnetron reactive sputtering under different Ar:O 2 ratios. The advantage of this deposited method is that it can deposit a CuO x thin film uniformly and rapidly with large scale. From the photoelectrochemical (PEC) properties of these CuO x photocathodes, it can be found that the CuO x photocathode with Ar/O 2 30:7 provide a photocurrent density of −3.2 mA cm −2 under a bias potential −0.5 V (vs. Ag/AgCl), which was found to be twice higher than that of Ar/O 2 with 30:5. A detailed characterization on the structure, morphology and electrochemical properties of these CuO x thin film photocathodes was carried out, and it is found that the improved PEC performance of CuO x semiconductor photocathode with Ar/O 2 30:7 attributed to the less defects in it, indicating that this Ar/O 2 30:7 is an optimized condition for excellent CuO x semiconductor photocathode fabrication.
No takes yet. Share an insight, caveat, or question.
Xie et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: