In order to study the interaction of calcium phosphate coatings with bone tissue, coated titanium cylinders with a standard size were implanted in dog femora. Coatings were made by plasma spraying powders of hydroxylapatite, beta-whitlockite, and tetracalciumphosphate particles. The plasma spraying process turns beta-whitlockite into alpha-TCP. Bone bonding and bone formation were evaluated by mechanical push-out tests and histological observations. Hydroxylapatite and tetracalciumphosphate coatings show an interface strength after 3 months of implantation of 34.3 +/- 6.5 MPa and 26.8 +/- 3.9 MPa, respectively, while alpha-TCP and blanco titanium lead to an interface strength of 10.0 +/- 3.5 MPa and 9.7 +/- 1.3 MPa, respectively. Histological examinations revealed that hydroxylapatite and tetracalciumphosphate give rise to an excellent bone formation, while alpha-TCP and blanco titanium evoked remodeling and less bone contact.
No takes yet. Share an insight, caveat, or question.
Klein et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: