The melting behavior of double crystalline poly(ε-caprolactone)- block -polyethylene (PCL- b -PE) copolymers, crystallized at various temperatures T c below the melting point of both blocks, has been investigated by time-resolved small-angle X-ray scattering with synchrotron radiation (SR−SAXS), conventional wide-angle X-ray diffraction (WAXD), and differential scanning calorimetry (DSC). The melting temperature of PCL blocks T m,PCL was ca. 56 °C and that of PE blocks T m,PE was ca. 96 °C, so that the PCL blocks melted first during heating followed by the melting of PE blocks. This melting behavior was unique when compared with that of crystalline homopolymers and crystalline−amorphous diblock copolymers. That is, the long period (LP) of the lamellar morphology, an alternating structure consisting of thin crystals and amorphous layers, decreased considerably at T m,PCL for PCL- b -PE crystallized at every T c investigated (22 °C < T c < 50 °C). Upon further heating from T m,PCL, LP decreased gradually for PCL- b -PE crystallized at higher T c (>40 °C) (h-PCL- b -PE) while it was constant for PCL- b -PE crystallized at lower T c (<40 °C). The morphology appearing in h-PCL- b -PE between T m,PCL and T m,PE was metastable, and the gradual decrease in LP during heating originated from the continuous rearrangement of the PE lamellar morphology facilitated by the melting of thinner PE crystals, which were previously formed by the crystallization of PCL blocks at T c .
No takes yet. Share an insight, caveat, or question.
Nojima et al. (2007) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: