Factors involved with the plasma-spray coating procedure, such as starting powder compound (fluorapatite, hydroxylapatite, magnesium-whitlockite, or tetra-calcium phosphate), powder particle distribution 1-45 or 1-125 microns), powder port gun (port 2 or 6), and post-heat treatment of 1 h at 600 degrees C, were examined for their effects on crystallinity and solubility/stability of the coating. From solubility tests, X-ray diffractometry, and scanning microscopy studies, the solubility and crystallinity were found to be dependent on Ca/P ratio, particle distribution, and post-heat treatment. The post-heat treatment influenced the degree of both crystallinity and solubility. The plasma-spray powder port factor for the hydroxylapatite coatings was not significant. Incubation in buffer of the coatings introduced precipitation at the surfaces of all non-heat-treated coatings except fluorapatite. No precipitation could be observed in any of the heat-treated coatings.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Klein et al. (1994) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: