The silver chloride-silver iodide equilibrium diagram has been constructed. The eutectic temperature is 259°C and the eutectic composition is 47 mole% silver chloride. The mean thermoelectric potential of this mixture between 260 and 960°C has been measured as -0·498 mv degK−1. Values of electrical conductivity of silver chloride-silver iodide mixtures are available in the literature, and the mean specific conductivity of the eutectic mixture between 260 and 960°C has been estimated as 2·91 Ω−1cm−1. The thermal conductivity has been measured as 1·83 × 10−3 W cm−1 degK−1 at 300°C. These values yield an approximate mean figure of merit for thermoelectric generation between 260 and 960°C of 0·4 × 10−3 degK−1. This is a threefold increase over the estimated figures of merit for the pure components.
No takes yet. Share an insight, caveat, or question.
Cornwell et al. (1969) studied this question.
Synapse has enriched 5 related papers. Consider them for comparative context:
More from Journal of Physics D Applied Physics