Answers are grounded in this paper and cite their sources.
The optical energy gap of amorphous Se powder has been determined by a photo-acoustic method and has been found to be 1.99+or-0.02 eV. On annealing, the gap decreases linearly as a function of annealing temperature towards that of the crystalline selenium.
No takes yet. Share an insight, caveat, or question.
Bhatnagar et al. (1985) studied this question.