High dielectric constant titanium dioxide thin films have been formed on silicon substrates by the rapid thermal oxidation of evaporated titanium. Oxidation of titanium at temperatures between 450 and 800 °C for periods of 1–60 s has been studied. Rutile polycrystalline layers of 800–2000 Å thickness were formed. Dielectric constants were in the range of 58–77 for titanium dioxide on silicon. High oxidization temperatures gave leakage currents of 10−7 A at 0.3 MV cm−1 for a 1500-Å-thick layer, and potential is seen for improved results with thinner layers.