An experimental unit was developed to allow the application of the glass specimen onto the metal surface at elevated temperatures and under controlled atmospheric conditions. Sodium disilicate glass on Armco iron had a contact angle of 55°± 2° at 900° to 1000° C. in vacuum and poor adherence; on magnetite, 2°± 1°, and excellent adherence. Behavior on oxidized iron was affected by the ability of the glass to dissolve large quantities of oxide rapidly. Glass when dropped onto a lightly oxidized surface spread toward lower angles and retracted essentially to the 55° angle on solution of the oxide; adherence, in this case, correspondingly ranged from good to poor. When the glass dissolved a sufficient amount of iron oxide and etching of the metal occurred, resulting in the appearance of fayalite, the contact angle was in the range 15° to 35° and the best adherence was obtained. Vaporization of iron in vacuum at 1000°C. did not seem to be retarded by thin oxide films.
No takes yet. Share an insight, caveat, or question.
Cline et al. (1961) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: