Samples of polysty re ne of an average m olec ular weight of abou t 230,000 an d weighin g 25 to 50 mg, were p y rolyzed in a vac uum of 10-6 mm of m ercury at 350 0 to 420 0 C. Tim e of pyroly is vari ed from 0.5 to 4 hoLll's. Th e fo ll owing fractions were obtain ed: (J) A so li d residue ha\' ing an average m olecular we ight of 2,182, (2) a wax-like fractio n con istin g of a mixtu re of a dimer, t rime r, a nd tetramer of styre ne, with a n average molec ula r weig ht of 264, (3) a liquid fraction co ns is t in g of 94.3 mole perce nt o f st ~' [' e n e , 5.6 mole pe rcent of to lu en e, and traces of eth yl benzene a nd m ethyl sty rene, (4) a ga eo us fraction consist in g mainl y of carbon monoxid e. Composit ion of a ll fractions and r elative amounts of t he wax-li ke and liquid fr actions were found to be inde penden t of time a nd temperat ure of pyrolysis, or of the a moun t of t he origin a l sample of po lystyrene. A maximum y ield of styrene, amount in g to 42 wei g ht pe rcent of the ori g in a l samp le of polys tyrene, was obtain ed at 420 0 C. The fact that on ly small fr agm ents, not la rger than the tet rame r, were vo lat i li zed, leads to t he co nclusion that th e larger f ragmen ts remai 11 e n tangled in t he mass of m acromolec ul es anel break up into smaller fragments, which t hen vo latili ze .
No takes yet. Share an insight, caveat, or question.
Madorsky et al. (1948) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: