According to Takezawa et at. , the thermoelectric power \(S\) along the basal plane in a synthetic single crystal graphite exhibits a sharp negative dip at T =35°K and a positive peak centered at 120°K. Subtracting the diffusion component \(Sd\) by use of an appropriate assumption, they have separated the phonon drag contribution \(Sₚ\) from \(S\). To get a theoretical explanation for \(Sₚ\), coupled Boltzmann equations for carriers and phonons are solved on the basis of a simplified ellipsoidal band model. The calculated \(Sₚ\) is proportional to T -3 above the dip temperature T d (35°K) and at T < T d it tends to zero as T 2∼4 with decreasing temperature. These behaviors are in qualitative agreement with the observed result.