This is the authors' abstract. We don't add key points for this paper.
Multiple-energy box profile elevated-temperature (700 °C) phosphorus ion implantations were performed into 4H–SiC in the doping range of 1×1017–1×1020 cm−3. The implanted material was annealed at 1500, 1600, or 1650 °C with an AIN encapsulant to prevent degradation of the SiC surface. Within this temperature range the sheet resistance does not change significantly for a given dose. The percentage of electrical activation of the P donors initially decreased with increasing implant dose for P-implant concentration up to 3×1019 cm−3 and then increased again at higher doses. For 1×1020 cm−3 P implant, a carrier concentration of 4×1019 cm−3 was measured at room temperature. In the 1017 cm−3 P doping concentration range substitutional activation greater than 85% was measured. Despite performing the implants at 700 °C, a significant amount of as-implanted damage was observed in the Rutherford backscattering (RBS) spectrum, even for 1018 cm−3 range P implantations. The RBS yield after annealing is near the virgin level for P concentrations up to 1×1019 cm−3, but above this concentration the RBS yield is above the virgin level, indicating a significant amount of residual lattice damage in the crystal.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Handy et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: