MCM-41 periodic mesoporous silicates were synthesized using cetyltrimethylammonium bromide, and their pore sizes were tailored by postsynthesis hydrothermal treatment method of Khushalani et al., allowing us to obtain large-pore MCM-41 samples with a high degree of structural ordering. It was shown that the pore size enlargement was accompanied by a significant improvement of pore size uniformity, a gradual decrease of the specific surface area, and the pore wall thickening. After a certain upper limit of pore size (i.e., about 6.5 nm) was reached, a further hydrothermal treatment led to samples of diminished quality. The structural uniformity decreases dramatically, i.e., the pore size distribution becomes broader and a small but noticeable amount of micropores develops. Moreover, the appearance of pore blocking effects (as inferred from the irreversibility of nitrogen adsorption−desorption isotherms) indicates that the pore geometry deviates significantly from its initial cylindrical shape characteristic for MCM-41 materials. The current study confirmed previous findings that the hydrothermal restructuring method is a convenient way to synthesize high quality MCM-41 silicates with tailored pore sizes, but only up to 6.5 nm.
No takes yet. Share an insight, caveat, or question.
Sayari et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: