We have manufactured a highly conductive and stretchable composite by backfilling a preformed graphene/MWCNT aerogel with poly(dimethylsiloxane) (PDMS). The electrical conductivity of our product can reach 2.8 S cm(-1) with only 1.3 wt% graphene/MWCNT loading, and remains constant after 100 times repeated stretching by 20% and 5000 times bending.