Carrier distribution in 150 keV, 10 16 /cm 2 75 As + ‐implanted Si layer after steam oxidation in the 850°–1000°C temperature range has been measured by the spreading‐resistance probe technique. When the oxidation temperature is below 1000°C, the carrier distribution shifts toward the surface at the initial stage of oxidation due to the Si ‐ SiO 2 interface movement, and sheet resistance increases correspondingly. After the initial stage, the carrier distribution then spreads gradually, corresponding to a slowing down in the oxidation rate. In contrast, when the oxidation temperature is above 1000°C, As diffusion effects dominate, and the carrier distribution spreads into Si and sheet resistance decreases monotonically with increasing oxidation time. These behaviors have been explained by simple numerical calculations.