In view of high catalytic activity and oxygen vacancy concentration, Ruddlesden–Popper (R-P) structure oxide has been widely used as the electrode material for solid oxide fuel cells (SOFCs). Herein, three R-P structure oxides, Pr 2– x Sr x Ni 0.2 Mn 0.8 O 4 ( x = 1, 1.2, and 1.5), are used as the semiconductor materials of single-component cells. The materials for the oxygen side are hybrid oxides consisting of R-P structure oxide and perovskite oxide. The hydrogen side was exposed to the reduction atmosphere before the test, and the perovskite structure disappeared and the lattice parameters of the R-P structure changed, resulting in the formation of a new R-P structure and MnO 2 or NiMn alloy. In addition, Pr 0.5 Sr 1.5 Ni 0.2 Mn 0.8 O 4 and reduced Pr 0.5 Sr 1.5 Ni 0.2 Mn 0.8 O 4 exhibit the most content of oxygen vacancy. For a single-component fuel cell (SCFC), the cell performance increased with the decrease in Pr content. The SCFC composed of Pr 0.5 Sr 1.5 Ni 0.2 Mn 0.8 O 4 shows the highest maximum power densities ( P max ), which reached 206.6 mW cm –2 at 700 °C. It is because the reduced Pr 0.5 Sr 1.5 Ni 0.2 Mn 0.8 O 4 has the highest catalytic activity for hydrogen oxidation reaction (HOR). Furthermore, the P max at 700 °C can reach a value of 198.1 mW cm –2 in SOFC mode, and in the case of SOEC mode, the current density at 700 °C is as high as −390.8 mA cm –2 with an applied electrolysis voltage of 1.3 V for the reversible single-component cell (RSCC) with Pr 0.5 Sr 1.5 Ni 0.2 Mn 0.8 O 4 as the semiconducting electrocatalyst.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Li et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: