Answers are grounded in this paper and cite their sources.
A small signal a‐c impedance method has been applied to the cell surface area carbon, in which the carbon electrode acts as a nonpolarizable electrode. Tungsten trioxide films were prepared by vacuum evaporation onto tin oxide covered glass substrate. The films, which were initially amorphous, were heated in air at temperatures from 300° to 400°C. The a‐c impedance measurements were carried out at several temperatures as a function of frequency from 10 −2 to 10 5 Hz. The Randles circuit was fitted to the data by nonlinear chi‐squared minimization. The amorphous films have higher diffusion coefficients, i.e. , about at 20°C, than crystalline samples, i.e. , at 20°C. The activation energy for the amorphous sample is about 0.25 eV as compared to about 0.4 eV for crystalline films. Such a difference might be explained by a difference in composition and density between the amorphous and crystalline films or by different transport mechanisms such as hopping of H + and diffusion of oxygen ion vacancies. The diffusion coefficient does not change significantly with composition in the range . The data suggest that may act as a nonblocking electrode with an exchange current density as high as 0.02 A · cm −2 .
No takes yet. Share an insight, caveat, or question.
Randin et al. (1982) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: