Answers are grounded in this paper and cite their sources.
Thermal stabilities of the colored forms at 80°C and photochemical fatigue resistances against coloration–discoloration cycles were measured in PMMA thin film, using 14 derivatives of fulgide with different heterocyclic structures. The indolyl (12), oxazolyl (13), and thiazolyl (14) derivatives showed very low thermal degradabilities (TD≤1.5%/day) while 12 and pyrazolyl derivative (9) showed low photochemical fatigues (PF≤0.2%/cycle), as compared with the furyl (1), thienyl (2), and pyrrolyl (3) derivatives. However, many of them featured low photo-responsiveness and low absorptivities for coloration on UV irradiation.
No takes yet. Share an insight, caveat, or question.
Kaneko et al. (1988) studied this question.