A preparation method for gadolinium compound (GdC) nanoparticles coated with silica ( GdC/SiO₂ ) is proposed. GdC nanoparticles were prepared with a homogeneous precipitation method at 80∘C using 1.0×10⁻³ M Gd(NO₃)₃ , 0.5 M urea and 0-3.0×10⁻⁴ M ethylenediarinnetetraacetic acid disodium salt dihydrate (ETDA) in water. As a result of preparation at various EDTA concentrations, GdC nanoparticles with a size as small as 40.5±6.2 nm, which were colloidally stable, were prepared at an EDTA concentration of 2.0×10⁻⁴ M. Silica-coating of the GdC nanoparticles was performed by a St ö ber method at 35∘C using 1.0-10.0×10⁻³ M tetraethylorthosilicate (TEOS), 11 M H₂O and 1.5×10⁻³ M NaOH in ethanol in the presence of 1.0×10⁻³ M GdC nanoparticles. Performance of preparation at various TEOS concentrations resulted in production of GdC/SiO₂ particles with an average size of 106.1±11.2 nm at a TEOS concentration of 5.0×10⁻³ M. The gadolinium (Gd) concentration of 1.0×10⁻³ M in the as-prepared GdC/SiO₂ particle colloid solution was increased up to a Gd concentration of 0.2 M by concentrating with centrifugation. The core-shell structure of GdC/SiO₂ particles was undamaged, and the colloid solution was still colloidally stable, even after the concentrating process. The concentrated GdC/SiO₂ colloid solution showed images of X-ray and magnetic resonance with contrast as high as commercial Gd complex contrast agents.
No takes yet. Share an insight, caveat, or question.
Kobayashi et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: