ZrO 2 –3 mol% Y 2 O 3 „single‐crystal” thin films with multiple variants were epitaxially formed on (100) cubic zirconia substrates. The films were prepared by spin‐coating an aqueous zirconium acetate/yttrium nitrate solution onto the cubic zirconia substrates and subsequently heat‐treated at temperatures between 1100° and 1400°C. Electron diffraction and dark‐field TEM observations showed that the film has tetragonal symmetry and consists of 50–100 nm variants with their c‐axes aligned with one of the three substrate cube axes. Unrelaxed strain energy estimates indicate that the two variants with their c 1 ‐axis parallel to the substrate/thin film interface are energetically favorable.