This is the authors' abstract. We don't add key points for this paper.
The initial rate of polymerization of highly purified styrene in bulk has been measured dilatometrically at 38.4, 56.4 and 70.1°C. For conversions up to one per cent a well‐reproducible rate was observed for samples handled in complete absence of atmospheric gases. For samples saturated with air an equally reproducible, though higher rate, was observed initially. The duration of this higher rate decreases with increasing length of storage between saturation and measurement. After polymerization at higher rate, the sample continues to polymerize at the rate observed for the air‐free samples.