Cerium-substituted YIG (YCeIG) films were grown on (111) oriented GGG substrates from PbO/B2O3 = based fluxes using the liquid phase epitaxy method. R5 parameter value about ten times as large as the usual one was used to increase the amount of the cerium entering the crystal. The Faraday rotation spectra were measured in the visible region (0.5~0.9μm) at room temperature. It was found that the Faraday rotation increased in the region between 0.65 and 0.85μm due to the cerium ion incorporated into the garnet films.