Answers are grounded in this paper and cite their sources.
We present strategies to improve low open-circuit voltage (Voc) for ZnO-poly(3-hexylthiophene) (P3HT) photovoltaic devices, which are typically ≤0.4 V, but vary among different reports. One factor affecting Vocvariability is the ZnO bandgap (Eg), which depends on detailed processing conditions. By decreasing the pyrolysis temperature of sol-gel ZnO films, we increased the ZnO Egby 0.14 eV and Vocof corresponding bilayer devices by 0.1 V. This is understood as increased donor-acceptor energy-level offset. Next, we demonstrate significant enhancement in Vocby depositing conformal amorphous TiOxfilms at the surface of planar ZnO films and ZnO nanorod arrays using a spin-coating method. The TiOxcoatings monotonically increased Vocfrom 0.4 to 0.8 V for devices with increasing TiOxthicknesses from 0 to ≥50 Å. Dark current-voltage measurement reveals that the TiOxcoating significantly decreases the reverse-bias current density, leading to an improvement in Voc, in excellent agreement with predictions from the modified ideal diode equation. This is consistent with passivation of ZnO surface defects by TiOx. In short, by varying the solution processing conditions, we modify the bulk and interfacial properties of the metal oxide acceptor, thus leading to systematic improvement in open-circuit voltage.
No takes yet. Share an insight, caveat, or question.
Lee et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: