This is the authors' abstract. We don't add key points for this paper.
Various biomedical applications of biodegradable nanofibers are a hot topic, as evidenced by the ever-increasing number of publications in this field. However, as-prepared nanofibers suffer from poor cell adhesion, so their surface is often modified. In this work, active polymeric surface layers with different densities of COOH groups from 5.1 to 14.4% were successfully prepared by Ar/CO2/C2H4 plasma polymerization. It has been shown that adhesion and proliferation of mesenchymal stem cells (MSCs) seeded onto plasma-modified PCL nanofibers are controlled by the CO2:C2H4 ratio. At a high CO2:C2H4 ratio, a well-defined network of actin microfilaments is observed in the MSCs. Nanofibers produced at a low CO2:C2H4 ratio showed poor cell adhesion and very poor survival. There were significantly fewer cells on the surface, they had a small spreading area, a poorly developed network of actin filaments, and there were almost no stress fibrils. The maximum percentage of proliferating cells was recorded at a CO2:C2H4 ratio of 35:15 compared with gaseous environments of 25:20 and 20:25 (24.1 ± 1.5; 8.4 ± 0.9, and 4.1 ± 0.4%, respectively). Interestingly, no differences were observed between the number of cells on the untreated surface and the plasma-polymerized surface at CO2:C2H4 = 20:25 (4.9 ± 0.6 and 4.1 ± 0.4, respectively). Thus, Ar/CO2/C2H4 plasma polymerization can be an excellent tool for regulating the viability of MSCs by simply adjusting the CO2:C2H4 ratio.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Manakhov et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: