This is the authors' abstract. We don't add key points for this paper.
A new atomic layer deposition (ALD) process for depositing nickel carbide (Ni 3 C x ) thin films is reported, using bis( N, N ′-di- tert -butylacetamidinato)nickel(II) and H 2 plasma. The process shows a good layer-by-layer film growth behavior with a saturated film growth rate of 0.039 nm/cycle for a fairly wide process temperature window from 75 to 250 °C. Comprehensive material characterizations are performed on the Ni 3 C x films deposited at 95 °C with various H 2 plasma pulse lengths from 5 to 12 s, and no appreciable difference is found with the change of the plasma pulse length. The deposited Ni 3 C x films are fairly pure, smooth, and conductive, and the x in the nominal formula of Ni 3 C x is approximately 0.7. The ALD Ni 3 C x films are polycrystalline with a rhombohedral Ni 3 C crystal structure, and the films are free of nanocrystalline graphite or amorphous carbon. Last, we demonstrate that, by using this ALD process, highly uniform Ni 3 C x films can be conformally deposited into deep narrow trenches with an aspect ratio as high as 20:1, which thereby highlights the broad and promising applicability of this process for conformal Ni 3 C x film coatings on complex high-aspect-ratio 3D architectures in general.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Guo et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: