Answers are grounded in this paper and cite their sources.
The electroreflectance of Cd x Hg 1- x Te alloys for x from 0 to 0.70 and for x =0.97 and x =1 was measured by the electrolyte technique in the range of photon energy 0.5 to 6 eV at room temperature. The E 0 + Δ 0 , E 1 , E 1 + Δ 1 and E 0 ' transitions were investigated as a function of alloy composition. The transition energies at critical points show quadratic dependence on the alloy composition. The deviations from linearity are interpreted by using the dielectric two band method. The spin-orbit splitting Δ 0 at k =0 for HgTe was measured directly as 1.08±0.02 eV at room temperature.
No takes yet. Share an insight, caveat, or question.
Moritani et al. (1973) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: