Aqueous suspensions of microfibrillated cellulose obtained by a high pressure homogenization process were freeze-dried after solvent exchange into tert-butanol. The resulting aerogels, which displayed a remarkable open morphology with a surface area reaching 100 m(2)/g, were subjected to a gas-phase esterification with palmitoyl chloride. Under these conditions, variations of the reaction temperature from 100 to 200 °C, of the reaction time from 0.5 to 2 h, and of the initial quantity of reagent, led to the preparation of a library of cellulose palmitates with DS varying from zero to 2.36. These products were characterized by gravimetry, FTIR, and (13)C solid-state NMR spectroscopy. Of special interest were the cellulose palmitate samples of low DS in the range of 0.1-0.4, which corresponded to hydrophobic cellulose microfibrils exclusively esterified at their surface while keeping intact their inner structure.
No takes yet. Share an insight, caveat, or question.
Fumagalli et al. (2013) studied this question.
Synapse has enriched 5 related papers. Consider them for comparative context: