Fine-grained bulk alloys with no crack in the 70:30 mol% Fe–Co system were prepared by means of shock compression of water-atomized powder and mechanical alloying (MA) treated ones. The grain size of the water-atomized bulk body was smaller (≤50μ m) than that of the molten bulk body (about 100μ m). The grain size decreased greatly with the MA treatment time, and ones for 21 h were estimated to be about 15 nm from the x-ray diffraction patterns. The coercivity value of the water-atomized bulk body was much larger than that of the molten bulk body. The coercivity value of the MA-treated bulk body increased with the MA treatment time, and then decreased, despite the very small grain size, probably due to the effect of ferromagnetic exchange interaction.