Laboratory batch and column tests were conducted to examine the reduction pathways and kinetics of N -nitrosodimethylamine (NDMA) by iron (Fe) and nickel-enhanced iron (Ni/Fe). A decrease in NDMA concentration and increases in dimethylamine (DMA) and ammonium were observed in both Fe and Ni/Fe columns. In the Fe column, the transformation process of NDMA appeared to follow pseudo-first-order kinetics with respect to NDMA, with an average half-life of 13±2 h. A small amount of nickel (0.25%) plated onto the iron greatly enhanced NDMA transformation rates. At early time the NDMA half-life in the Ni/Fe column was 2 min but as time progressed the half-life increased to 4 min, and departures from first-order kinetics were observed. The mass balances of carbon in DMA and nitrogen in DMA and ammonium improved over time and reached 100% and 90%, respectively, after NDMA had passed through the column for more than 50 pore volumes (PV). No 1,1-dimethylhydrazine, nitrous oxide, or methane were detected. Based on the electrochemical properties of NDMA, the transformation mechanism of NDMA with Fe and Ni/Fe is postulated to be catalytic hydrogenation, resulting in N−N bond breakdown to form DMA and ammonium as final products. Nickel, being a much stronger catalyst than Fe for catalytic hydrogenation, resulted in a much faster reduction rate of NDMA. Of several methods tested, flushing the Ni/Fe column with 0.01 N sulfuric acid proved to be the most effective in restoring the Ni/Fe activity. The rapid transformation rate on Ni/Fe and the formation of nontoxic products indicate that this material may be applicable for treating NDMA contaminated water, both in-situ and above ground.
No takes yet. Share an insight, caveat, or question.
Gui et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: