Raman scattering has been used to measure phonon linewidths and frequencies of a number of high quality diamond crystals. It was found that the defect induced broadening produced a Lorentzian line shape. The smallest Lorentzian linewidth of 1.68 cm−1 at 300 K caused by anharmonicity and defects was obtained for the high pressure synthesized diamond. The linewidths of the diamonds grown by chemical vapor deposition varied, with the best sample having a linewidth of 2.31 cm−1, close to the values for natural diamonds. No measurable phonon frequency shift caused by defects was found.