Answers are grounded in this paper and cite their sources.
Laminated (Fe97Al3)1-xNx/Ni81Fe19 films have been prepared by reactive RF-diode (RFD) and DC-magnetron (DCM) sputtering within a sputter machine developed for the production of magnetoresistive films. The thickness of the films was typically at ≈0.5 μm with a lamination period between 100 Å and 1200 Å and a thickness ratio tFeAlN/tNiFefrom 1 to 23. RFD sputtered films exhibit a high Bs (up to 20 kG) and excellent soft magnetic behaviour (Hc= 0.4 Oe, Hk =3 Oe, λs < 1*10-6) as long as the lamination period is below a few hundred Å. The thickness uniformity of the films is better than ±3%. Uniform N distribution was proven by RBS investigation. XRD measurements reveal a nanocrystalline structure of both sublayers for RFD and DCM sputtered films for a nitrogen concentration > 8 at%, without exhibiting significant differences between center and edge of the substrates. For films with DCM sputtered FeAlN sublayer, however, it was difficult to align the uniaxial magnetic anisotropy by the applied collinear magnetic field, particularly on larger substrates and at low nitrogen concentrations.
No takes yet. Share an insight, caveat, or question.
Maaß et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: