Laser beam shaping in PBF-LB/M modifies the spatial laser energy distribution, affecting melt-pool evolution, defect formation, and mechanical response. Ti-6Al-4V was processed using Gaussian, core–ring, and ring-dominated beam profiles. Measured beam maps were used to determine the effective beam diameter in a modified energy metric (VED M , J mm⁻² s⁻¹/²) for cross-mode comparison. Densification and pore characteristics were assessed in cubes and tensile specimens. Core–ring and ring-dominated profiles transitioned from lack-of-fusion defects at low input to near-full density at higher input, whereas Gaussian shifted toward keyhole-type porosity at the highest input. At VED M = 332 J mm⁻² s⁻¹/², the µCT-scanned tensile gauge regions showed lower relative density for Gaussian (~98.6%) than for core–ring and ring-dominated conditions (~99.8%). Tensile specimens produced with Gaussian and ring-dominated beams were tested at RT, 200 °C, and 400 °C. All conditions showed temperature-dependent softening. However, at high VED M and 400 °C, the ring-dominated condition retained higher ductility (~10%) than the Gaussian condition (~7%), while maintaining a comparable peak stress. Fractography showed pore-assisted initiation in the Gaussian condition and ductile tearing with pronounced necking in the ring-dominated condition. Overall, elevated-temperature tensile performance was primarily associated with pore type and severity, while VED M provides a practical framework for cross-mode comparison.
No takes yet. Share an insight, caveat, or question.
Ullah et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: