The aim of this study was to compare the shear bond strengths (SBS) of cast, machined, and laser-sintered titanium to dental porcelain. Two kinds of dental porcelains (Titankeramik and Triceram) were applied on cast (Tritan), machined (DC-Titan), and laser-sintered (EOSINT) titanium specimens (n=10). SBS test was conducted, and fracture surface analysis was also performed to determine the failure modes. Two-way ANOVA, Student's t-test, and post hoc test were used to analyze the data (p<0.05). Among the titanium specimens, the SBS values of laser-sintered titanium specimens were significantly higher than the machined and cast titanium specimens (p<0.01). Comparison of Triceram and Titankeramik veneering porcelains showed no statistically significant differences in SBS when they were applied on laser-sintered and cast titanium specimens (p>0.05). Specimens in all the test groups exhibited adhesive or combined failure, with the Titankeramik-machined titanium group exhibiting the highest adhesive failure rate (40%). Results showed that porcelain-titanium bond strengths could be improved by using the new laser sintering technique to produce titanium for prosthodontic applications.
No takes yet. Share an insight, caveat, or question.
İşerı et al. (2011) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: