Answers are grounded in this paper and cite their sources.
Pure titanium was cast into different ceramic moulds based on MgO/Zr, SiO2/ammonium phosphate and ZrO2 blends. A special casting technique was employed whereby liquid metal was poured under argon pressure into a mould which had been placed in a vacuum chamber. Mould temperatures selected were 20° and 800°C. Examinations included evaluation of external casting features, microstructure, EDS analysis, and microhardness adjacent to the casting surface. The type of microstructure was found to vary according to the mould material, consisting, in general, of an acicular alpha zone at the surface, with equiaxed grains towards the centre of the casting. The grain size and area fraction of the zones changed with mould types and temperature. The casting surface conditions were related to the metal/mould reaction. In general, the SiO2/ammonium phosphate mould, heated to 800°C, exhibited the most severe reaction with Ti, resulting in a thick reaction layer, with the formation of cracks and the evolution of gas (less severe with moulds at room temperature). Si and oxygen from the mould was found in the Ti in concentrations which decreased with distance from the surface. Microhardness values increased from 200 VHN at the centre of the casting to 500–800 VHN at the surface.
No takes yet. Share an insight, caveat, or question.
Wictorin et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: