Vapor formation in the ZnO–Nb2O5 system in the range 1223–1465 K was studied by Knudsen effusion mass spectrometry. Over the entire range of condensed phase compositions, the saturated vapor above the system consists of zinc atoms, oxygen molecules, and a small amount of ZnO molecules. The absolute component partial vapor pressures and activities were calculated. The р–х section of the global р–Т–х phase diagram at 1353 and 1443 K was plotted. The second-law and third-law values were determined of the standard enthalpies of selected heterophase reactions and the standard enthalpies of formation zinc niobates: Δ fH_298^∘ (Zn3Nb2O8) = –2992.0 ± 30.2 kJ/mol, Δ fH_298^∘ (ZnNb2O6) = –2292.4 ± 19.9 kJ/mol, and Δ fH_298^∘ (Zn2Nb34O87) = –33056.1 ± 15.0 kJ/mol, and their enthalpies of formation from simple oxides: (Zn3Nb2O8) = –50.0 ± 20.0 kJ/mol, (ZnNb2O6) = –40.5 ± 15.0 kJ/mol, and (Zn2Nb34O87) = –90.9 ± 15.0 kJ/mol.
No takes yet. Share an insight, caveat, or question.
Грибченкова et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: